[1]叶翠莲,乔智国,李腾飞,等.磨损套管剩余强度有限元分析[J].油气井测试,2020,29(03):6-10.[doi:10.19680/j.cnki.1004-4388.2020.03.002]
YE Cuilian,QIAO Zhiguo,LI Tengfei,et al.Finite element analysis of residual strength of worn casing[J].Well Testing,2020,29(03):6-10.[doi:10.19680/j.cnki.1004-4388.2020.03.002]
点击复制
磨损套管剩余强度有限元分析(
)
《油气井测试》[ISSN:1006-6977/CN:12-1485/TE]
- 卷:
-
29卷
- 期数:
-
2020年03期
- 页码:
-
6-10
- 栏目:
-
- 出版日期:
-
2020-06-25
文章信息/Info
- Title:
-
Finite element analysis of residual strength of worn casing
- 文章编号:
-
1004-4388(2020)03-0006-05
- 作者:
-
叶翠莲; 乔智国; 李腾飞; 张诗阳
-
中国石化西南油气分公司石油工程技术研究院 四川德阳 618000
- Author(s):
-
YE Cuilian; QIAO Zhiguo; LI Tengfei; ZHANG Shiyang
-
Research Institute of Petroleum Engineering Technology, Sinopec Southwest Oil and Gas Company, Deyang, Sichuan 618000, China
-
- 关键词:
-
套管强度; 有限元分析; 非线性屈曲分析; 磨损; 抗内压强度; 抗挤强度; 剩余强度; 屈曲特征值
- Keywords:
-
casing strength; finite element analysis; nonlinear buckling analysis; wear; internal pressure strength; collapsing strength; residual strength; buckling eigenvalue
- 分类号:
-
TE257
- DOI:
-
10.19680/j.cnki.1004-4388.2020.03.002
- 文献标志码:
-
A
- 摘要:
-
为计算磨损套管剩余强度,采用有限元分析方法,通过对标准套管进行屈曲分析求出特征值,引入特征值计算结果进行非线性分析,计算得到套管强度,并与API标准值进行对比,得到套管抗内压强度误差为0264%,抗外挤强度误差为0013%,验证了有限元分析方法的可行性和准确性;通过引入屈曲特征值进行磨损套管塑性变形分析,建立了磨损套管的剩余强度分析方法,对1937mm×127mmP110套管发生1mm、3mm和5mm月牙形磨损时套管剩余强度进行分析计算。DY7井实际应用表明,该计算结果可靠,能够满足后续作业对井筒承压能力的要求,为施工提供决策依据。
- Abstract:
-
To calculate the remaining strength of worn casing, using the finite element analysis method, we first calculated the eigenvalue of standard casing through buckling analysis, then conducted nonlinear analysis to estimate the casing strength, and compared with the API value, and finally we got the error of the internal pressure strength is 0264%, and the error of the external collapsing strength is 0013%. The results have proved that finite element analysis is effective and feasible. After introducing the buckling eigenvalue for plastic deformation of worn casing, we established a method for analyzing the residual strength of worn casing, and used it to analyze the residual strength of the P110 casing (127 mm, 1937 mm) with 1 mm, 3 mm and 5 mm crescent wears. Application in Well DY7 indicates that the calculated result is reliable, and can meet the requirements of subsequent operation on the pressure capacity of the wellbore. The result provided a basis for making the decision on subsequent operation.
备注/Memo
- 备注/Memo:
-
2020-01-10收稿,2020-04-20修回,2020-05-11接受,2020-06-20网络版发表
中国石油化工集团有限公司科技部科技攻关项目“深层页岩气高效钻完井技术”(P18058-2)
叶翠莲,女,1980年出生,硕士研究生,高级工程师,2006年7月毕业于成都理工大学应用数学专业,目前主要从事井下工具研发工作。电话:0838-2551110,18161308171;Email:156173080@qq.com。通信地址:四川省德阳市龙泉山北路298号石油工程技术研究院,邮政编码:618000。